Weld Metal Chemical Analysis ( % ) | |||||||
C | Si | Mn | Mo | P | S | ||
Wire ( S3Mo ) | 0.07 – 0.10 | Max 0.10 | 1.35- 1.65 | 0.5-0.6 | Max 0.03 | Max 0.03 | |
KJS-125 ( S3Mo) + KJF – 910 | 0.04 – 0.06 | 0.2 – 0.3 | 1.2 – 1.4 | 0.5-0.6 | Max 0.03 | Max 0.03 | |
KJS-125 ( S3Mo) + KJF – 915 | 0.05 – 0.08 | 0. 5 – 0.6 | 1.70 – 1.90 | 0.5-0.6 | Max 0.03 | Max 0.03 |
Weld Metal Mechanical Properties | ||||||
Wire + Flux | U.T.S. | Y.T.S. | EL | Charpy test | ||
( Mpa) | ( Mpa) | (%) | RT | -30 °C | -40°C | |
KJS-125 ( S3Mo) + KJF – 910 | 585 – 615 | 490 – 510 | 20 – 22 | 60- 80 | 35 – 45 | — |
KJS-125 ( S3Mo) + KJF – 915 | 640 – 660 | 550 – 570 | 19- 21 | 50 – 65 | 30 – 40 | — |
Wire Diameter and Packing |
Packing: In Drum of 350 – 450Kgs, Coil of 25Kgs or Spool of 15Kgs according to below details at customer’s option
Wire Dia (mm) | Packing |
1.60 – 2.40 | 15Kgs Spool |
2.40 – 3.20 – 4.0 – 5.0 | 25Kgs Coil and Drum |
Advantages |
Cupper Coated Wire, Suitable for Submerged Arc Welding of Low Alloy and C-Mn Steel
Suitable for submerged arc welding of a series of steels including Molybdenum, high strength, fine grain and low temperature ones.
Current: DCEP/AC