Weld Metal Chemical Analysis ( % ) | |||||||
C | Si | Mn | Mo | P | S | ||
Wire ( S2Mo ) | 0.06 – 0.10 | Max 0.10 | 0.85 – 1.05 | 0.4-0.5 | Max 0.03 | Max 0.03 | |
KJS-124 ( S2Mo) + KJF – 610 | 0.04 – 0.06 | 0.35 – 0.45 | 1.55 – 1.75 | 0.4-0.5 | Max 0.03 | Max 0.03 | |
KJS-124 ( S2Mo) + KJF – 614 | 0.04 – 0.06 | 0.25 – 0.35 | 1.65 – 1.9 | 0.4-0.5 | Max 0.03 | Max 0.03 |
Weld Metal Mechanical Properties | ||||||
Wire + Flux | U.T.S. | Y.T.S. | EL | Charpy test | ||
( Mpa) | ( Mpa) | (%) | RT | -30 °C | -40°C | |
KJS-124 ( S2Mo) + KJF – 610 | 570 – 600 | 470 – 490 | 23 – 25 | 90- 100 | 45 – 55 | 40 – 44 |
KJS-124 ( S2Mo) + KJF – 614 | 620 – 635 | 540 – 565 | 20- 22 | 65 – 80 | 40 – 450 | 30 – 35 |
Wire Diameter and Packing |
Packing: In Drum of 350 – 450Kgs, Coil of 25Kgs or Spool of 15Kgs according to below details at customer’s option
Wire Dia (mm) | Packing |
1.60 – 2.40 | 15Kgs Spool |
2.40 – 3.20 – 4.0 – 5.0 | 25Kgs Coil and Drum |
Advantages |
Cupper Coated Wire, Suitable for Submerged Arc Welding of Low Alloy and C-Mn Steel
Is used with KJF-610 for welding of fine grain steel
Is used with KJF-614 for welding different thickness of gas and oil pipe.
Current: DCEP/AC